Formation and influence factors of solid electrolyte interphase film on the negative electrode surface in lithium-ion batteries

Thumbnail
全文浏览
Formation and influence factors of solid electrolyte interphase film on the negative electrode surface in lithium-ion batteries.htm (468bytes)
发布日期
2005-09
作者
Ming-Sen Zheng
郑明森
Quan-Feng Dong
董全峰
Hui-Qun Cai
Ming-Gang Jin
Zu-Geng Lin
林祖赓
Shi-Gang Sun
孙世刚
所在专题
  • 化学化工-已发表论文 [14235]
显示详细条目
摘要
The electrochemical performance of a lithium ion battery depends basically on the characteristics of the solid electrolyte interphase (SEI) film that is formed on the negative electrode surface of the battery during its first charge-discharge process. The formation mechanism of the SEI film on surface of a MCF (mesophase-pitch-based carbon fiber) negative electrode was studied in the present paper. The studies have demonstrated the influence of some typical impurities on the formation of SEI film, and characterized the morphology and the composing of the SEI films using scanning electron microscopy and X-ray photoemission spectroscopy. The shape of SEI films overlaid on MCF has been observed distinctly. (c) 2005 The Electrochemical Society.
出处
JOURNAL OF THE ELECTROCHEMICAL SOCIETY,2005,152(11):A2207-A2210
本条目访问地址(URI)
https://dspace.xmu.edu.cn/handle/2288/10946

copyright © 2002-2016  Duraspace  Theme by @mire  厦门大学图书馆  
关于我们 | 相关政策
 

 

浏览方式

全部社群发布日期作者题名主题该专题发布日期作者题名主题

我的账号

登录注册

copyright © 2002-2016  Duraspace  Theme by @mire  厦门大学图书馆  
关于我们 | 相关政策