Show simple item record

dc.contributor.authorWeng, Wei-Zheng
dc.contributor.author翁维正
dc.contributor.authorPei, Xiao-Qing
dc.contributor.authorLi, Han-Mei
dc.contributor.authorLuo, Chun-Rong
dc.contributor.author罗春荣
dc.contributor.authorLiu, Ying
dc.contributor.author刘颖
dc.contributor.authorLin, Hai-Qiang
dc.contributor.author林海强
dc.contributor.authorHuang, Chuan-Jing
dc.contributor.author黄传敬
dc.contributor.authorWan, Hui-Lin
dc.contributor.author万惠霖
dc.date.accessioned2011-07-08T12:22:13Z
dc.date.available2011-07-08T12:22:13Z
dc.date.issued2006-07
dc.identifier.citationCATALYSIS TODAY,2006,117(1-3):53-61zh_CN
dc.identifier.issn0920-5861
dc.identifier.urihttp://dx.doi.org/doi:10.1016/j.cattod.2006.05.011
dc.identifier.urihttps://dspace.xmu.edu.cn/handle/2288/10023
dc.description.abstractComparative studies using high temperature in situ Raman spectroscopy, TPSR, pulsed reactions of CH4, H-2-TPR and O-2-TPD techniques were carried out on Rh/Al2O3 calcined at 600 and 900 degrees C to elucidate the effect of calcination temperatures on the nature of the Rh species in the catalysts and its relationship with the catalytic performance of Rh/Al2O3 for partial oxidation of methane (POM) to synthesis gas. The results indicate that significant difference in the POM performance of Rh/Al2O3 catalysts calcined at 600 and 900 degrees C can be attributed to the formation of rhodium species of different nature after the samples were calcined in the air at above temperatures. Calcining a Rh/Al2O3 sample in the air at 900 degrees C caused not only the formation of more than 81% of rhodium species irreducible by H-2 at the temperature below 600 degrees C, but also affected the redox property of the RhOx species reducible at the temperature below 250 degrees C. Compared to the rhodium species in the Rh/Al2O3 calcined at 600 degrees C, those in the catalyst calcined at 900 degrees C possesses stronger Rh-O bonds and higher oxygen affinity. These factors would affect the concentration of oxygen species on the two catalysts under the POM reaction conditions and consequently affect the primary products of the reaction. The results of TPSR and in situ Raman characterizations on the POM reaction over the catalysts indicate that, Rh/Al2O3 in fully oxidized form are mainly responsible for complete oxidation CH4 to CO2 and H2O. The catalysts abruptly changed its oxidation state at the temperature when POM reaction starts. The results of high temperature Raman characterizations also suggest that a rhodium species in which Rh may substitute for the At site of Al2O3 was formed in the Rh/Al2O3 sample calcined in air at 900 degrees C. This rhodium species is difficult to be reduced to Rh metal by H-2 at temperature below 600 degrees C. (C) 2006 Elsevier B.V. All rights reserved.zh_CN
dc.language.isoenzh_CN
dc.publisherELSEVIER SCIENCE BVzh_CN
dc.subjectmethane partial oxidationzh_CN
dc.subjectsynthesis gaszh_CN
dc.subjectRh/Al2O3zh_CN
dc.subjectcalcination temperaturezh_CN
dc.subjectreaction mechanismzh_CN
dc.subjectin situ Ramanzh_CN
dc.titleEffects of calcination temperatures on the catalytic performance of Rh/Al2O3 for methane partial oxidation to synthesis gaszh_CN